NanoXact Gold Nanospheres – PVP (Dried)·

Nanoparticle powder, specifically formulated to maintain the nanoparticles’ unique properties – no aggregation! Powder format allows greater flexibility with solvent choice and concentration. See list of compatible solvents ❯

Polyvinylpyrrolidone (PVP) helps maintain stability when particles are deposited onto a substrate or thin film. Learn more ❯

NanoXact materials are high quality, unagglomerated and monodisperse nanoparticles. Learn more ❯

Need particles for conjugation? See BioReady Gold.

Need particles for in-vivo or in-vitro studies? See BioPure Gold.

Select Diameter
Select Mass

Product number: AUPD5-1MG

Continue Shopping or View Cart
  Last Call – Discontinued and premium one-off products offered at reduced prices

Specifications & CoA

TEM Diameter Size Distribution (CV) Example Certificate of Analysis
(How do I read this?)
5 nm ± 1 nm ≤ 18% Download Example CoA
7 nm ± 2 nm ≤ 12% Download Example CoA
10 nm ± 2 nm ≤ 12% Download Example CoA
15 nm ± 3 nm ≤ 12% Download Example CoA
20 nm ± 3 nm ≤ 15% Download Example CoA
30 nm ± 3 nm ≤ 15% Download Example CoA
40 nm ± 4 nm ≤ 15% Download Example CoA
50 nm ± 4 nm ≤ 15% Download Example CoA
60 nm ± 4 nm ≤ 15% Download Example CoA
70 nm ± 5 nm ≤ 15%
80 nm ± 5 nm ≤ 15% Download Example CoA
100 nm ± 5 nm ≤ 15% Download Example CoA

Note: approximate ranges below are dependent on diameter

  • Particle surface: PVP
  • Particle form: powder
  • Peak wavelength (λmax), when redispersed: 510 to 565 nm